Standard:API 5L PSL1|PSL2.
Scope:API 5L is generally refers to the standards of pipeline steel, include pipeline pipe and pipeline steel plate.
API 5L line pipe steel grade levels:GR. B, X42, X46 and X52, X56, X60, X70 and X80.
Details

Looking to the future, our company will make its main business more competitive while carrying out diversified, extensive, green and harmonious development modes, so as to be the most competitive API 5L PSL1 X42 pipeline producer in the world as well as a worldwide first-class enterprise. With ten years cooperation with these big mills, now we are the agent of super stainless steel mills in China.

We have a stable system and professional human resource management work as the support, from the six aspects of guidance, cohesion, incentive, constraint, radiation and stability, we continue to introduce, modify and train employees from concept to action, and shape employees through constant guidance of common values.

API 5L PSL1 X42 pipeline, Medium and heavy steel plate is a kind of steel plate with outstanding characteristics. First of all, there are many kinds of thickness of medium and heavy steel plate, which are generally relatively thick. Secondly, the thickness of medium and heavy steel plate is relatively thick, so it can be used for high strength application such as bridges. Thirdly, the corrosion resistance and wear resistance of medium and heavy steel plate are much better than ordinary steel plate.

The main function of boron in API 5L PSL1 X42 pipeline and so on steel is to increase the hardenability of steel, so as to save other rare and precious metals, such as nickel, chromium and molybdenum. For this purpose, the boron content is generally regulated in the range of 0.001% - 0.005%. It can replace 1.6% nickel, 0.3% chromium or 0.2% molybdenum. It should be noted that molybdenum can prevent or reduce temper brittleness, while boron slightly promotes temper brittleness, so molybdenum can not be completely replaced by boron.


If you need a quotation, please send us your detailed requirements and we will reply to you within 24 hours.

Your Name *
Email
Message
    
ul>

Location

Home > News>

What are the requirements for welding thick api 5l psl1 x42 pipeline

Standard:API 5L PSL1|PSL2.
Scope:API 5L is generally refers to the standards of pipeline steel, include pipeline pipe and pipeline steel plate.
API 5L line pipe steel grade levels:GR. B, X42, X46 and X52, X56, X60, X70 and X80.
Details

Looking to the future, our company will make its main business more competitive while carrying out diversified, extensive, green and harmonious development modes, so as to be the most competitive API 5L PSL1 X42 pipeline producer in the world as well as a worldwide first-class enterprise. With ten years cooperation with these big mills, now we are the agent of super stainless steel mills in China.

We have a stable system and professional human resource management work as the support, from the six aspects of guidance, cohesion, incentive, constraint, radiation and stability, we continue to introduce, modify and train employees from concept to action, and shape employees through constant guidance of common values.

API 5L PSL1 X42 pipeline, Medium and heavy steel plate is a kind of steel plate with outstanding characteristics. First of all, there are many kinds of thickness of medium and heavy steel plate, which are generally relatively thick. Secondly, the thickness of medium and heavy steel plate is relatively thick, so it can be used for high strength application such as bridges. Thirdly, the corrosion resistance and wear resistance of medium and heavy steel plate are much better than ordinary steel plate.

The main function of boron in API 5L PSL1 X42 pipeline and so on steel is to increase the hardenability of steel, so as to save other rare and precious metals, such as nickel, chromium and molybdenum. For this purpose, the boron content is generally regulated in the range of 0.001% - 0.005%. It can replace 1.6% nickel, 0.3% chromium or 0.2% molybdenum. It should be noted that molybdenum can prevent or reduce temper brittleness, while boron slightly promotes temper brittleness, so molybdenum can not be completely replaced by boron.